    Isolating bindings from Titanal board.

    I know there has been some considerable discussion about bindings on titanal boards lately, but i'm still trying to wrap my head around one thing in particular. Wouldn't lexan risers alter the overall flex of the board? Or is it not considerable? I see the Sflex comes with different stiffnesses, but i'm looking for something cheap (i.e. homemade). So in effect, I'm looking for any input from those that use lexan/plexiglass/other under their bindings.

    Thanks in advance.
    Last edited by cail; November 5th, 2007 at 11:15 AM. Reason: clarification

  2. #2
    Join Date
    Nov 2003
    Location
    toronto, ontario, canada
    Posts
    773

    S-Flex

    Quote Originally Posted by cail
    ... I see the Sflex comes with different stiffnesses, ...
    Where did you 'see' this information?

    Edit: Found the info in another thread here where Bola made reference to various stiffness of S-Flex. That was only on pre-production/prototype versions. The production models that are available now only come in one configuration.
    Last edited by yyzcanuck; November 5th, 2007 at 10:03 AM.
    .
    Join our email list HERE
    .
    Eventus stultorum magister.

  3. #3
    Join Date
    Jan 2007
    Location
    Albany, NY
    Posts
    667
    interesting... yeah that was the same post i was referring to. in that case, how stiff are Sflex compared with Hangl plates and Kessler risers?

    i'm only interested cause I'm going to make my own plates, but i dont want to go with straight lexan cause i'd think it would be too stiff, so maybe a combination of materials that won't be too soft but still able to flex with the board.

  4. #4
    Join Date
    Nov 2003
    Location
    Layton, UT
    Posts
    778

    Similar question

    Quote Originally Posted by cail
    Wouldn't lexan and plexiglass risers alter the overall flex of the board? Or is it not considerable?
    From what I've gathered, these lexan/plexiglass etc. plates are in the 4-5mm (??) range for thickness. From what I know about lexan, it has a high impact strength as well as a certain elasticity. One would think this would allow the material to flex with the board. Would like to hear other's experience with this as well.

  5. #5
    Join Date
    Nov 2003
    Location
    Big Utah country in them hills
    Posts
    1,431

    ok lets try this

    Most metal board that fail, fail due to several factors however one of the safe guards all metal board riders should apply is a “distribution plate” between the board and topsheet . Every binding make a pressure point where it makes contact at the beginning of the flex pattern. I.E. at the first point the binding limits the board flex regardless of the binding this is going to happen. What happens is as the board bends and rebounds it can “dent” the metal creating a weak spot in the shear strength the metal creates, weakening the board at that point and possibly failing later. Using Plex under the binding stops the Dent from happening and helps the binding flex point be distributed over more area and since the plex is soft it doesn’t make the hinge point like the binding does (nor does it change board feel). In till the hangle plate most athletes on metal board were riding plex “pads” under there bindings.
    However it is very rare to see Bombers or Cateks under racers feet. Most choose a softer binding for there metal rides. But even with bindings like F2s or burtons boards were breaking left and right and we where really getting nervous on them but the ride was so much better you really could not be competitive on none metal boards. But when metal came out to the masses it became obvious some binding where much more abusive to metal boards, some manufactures even claimed warranties would be voided if you used some brands of bindings on their metal stick.

    I think we are going to make some plates from products you can get at Home Depot for around 10 dollars a pair and post a how to on the hardbooter site in the next few days. Perhaps even a template you can print and use, I will also post some photos of a broken metal board that clearly shows the pressure point fracture. That then led to me breaking my back and ending my racing career

    Since metal boards are finding there way into the hands of so many recreational riders who clearly don’t want to take the risk of a board breaking do to pressure point failure I highly recommend installing the plates on any board with exposed or covered metal in the product. Plus you still get some added lift to help with leverage.

    With some bindings you may still want to take added measures using the suspension kits for bombers and the extra D3 thing for cateks. With the Plex pad

    I also try and educate riders on metal boards about the new feel of metal under there feet and encourage all metal board riders to try softer boots and bindings if they have the chance. Most new school metal board do not have to be as stiff to provide a bad ass ride so neither does the gear need to “power” it properly unlike superboards of the past.

    I also am straight afraid to use one particular brand of bindings on metal boards due to personally watching several boards fail (metal and wood) with this binding. All from pressure point issues with this particular binding. It may be due to the lack of suspension pads under the binding it may also be due to the direct metal to metal contact when mounted, perhaps its because the milled holes are not round and “strange” torque is introduced into the mounting points in some cases, causing the binding to A damage inserts or B rip out of the board while riding some times due to damaged inserts from mounting or perhaps since the screw provided with the binding may not have enough length to make proper purchase. Also this brand of binding always leaves marks on the topsheet of boards and causes dents in metal under and around the binding after only a single run.
    Hardbooter.com



    “Yes, it is much more challenging to ski 210 cm toothpicks. But do you choose to go to the wooden outhouse in the wintertime? Or it is more pleasant to use the indoor toilet instead? Why take challenges from the past when we can go on and challenge us on what’s possible with the current technology?”

    Shane McConkey disscussing rockered skis.

  6. #6
    Join Date
    Sep 2005
    Location
    Hell
    Posts
    3,672
    bordy = succinct!
    If death leads to eternal bliss why are you wearing a seatbelt?

  7. #7
    Join Date
    Jan 2005
    Location
    Vancouver, BC, Canada
    Posts
    4,354
    Bordy,
    I really think you should refrain from calling the pads Plex. It gives the wrong impression that they should be made out of Plexiglass (acrylic) insead of Lexan (polycarbonate). As discussed before, Plexiglass is a brittle material, it shatters and doesn't like compression loads araund drilled holes, nor tightening with the screws.
    Lexan or other polycarbonates are flexier and practically indestructable.

    On the side note, did anyone try the cutting board (high-molecular polyethilene). It should have nice dumping properties too...
    INSTRUCTION | CASI L2 - hard boots all the way! | Vancouver Carvers' Diaries 2012/13 | Items for sale

  8. #8
    Join Date
    Dec 2005
    Location
    Roseville, MN
    Posts
    1,238
    It is actually a buckling beam problem.
    Even stress distribution over the length of a beam can be disrupted by surface imperfections and irregularities. If a beam has a "dent" it will have a stress concentration a this point, being a small feature, the stress concentration is VERY high. With this flaw the beam may have been able to handle a much higher stress than it will after the flaw is created.

    Or something like that.....

    My question is: Why don't the manufactures supply boards with a floating plate (hangl plate) already attached? Then you just bolt on your binding of choice and away you go. Ski manu's have been doing this for quite a while.
    Doug in MN

  9. #9
    Join Date
    Nov 2003
    Location
    Layton, UT
    Posts
    778
    Quote Originally Posted by Bordy
    I think we are going to make some plates from products you can get at Home Depot for around 10 dollars a pair and post a how to on the hardbooter site in the next few days. Perhaps even a template you can print and use, I will also post some photos of a broken metal board that clearly shows the pressure point fracture.
    Look forward to this!!

    What kind of thicknesses have you used?

  10. #10
    Join Date
    Feb 2004
    Location
    Osburn, Idaho
    Posts
    1,757

    cutting board

    I've been wondering about using cutting board material as well.I have a couple of poyethelene ones and even put them in the freezer for a day to test for brittleness and they seemed fine.This is just the kind of redneck engineering that I apply to most of my ideas/tweaks so I plan to give it a try.

  11. #11
    Join Date
    Nov 2003
    Location
    The moose's maw rangeley, me
    Posts
    6,178
    Quote Originally Posted by MUD
    It is actually a buckling beam problem.
    Even stress distribution over the length of a beam can be disrupted by surface imperfections and irregularities. If a beam has a "dent" it will have a stress concentration a this point, being a small feature, the stress concentration is VERY high. With this flaw the beam may have been able to handle a much higher stress than it will after the flaw is created.

    Or something like that.....

    My question is: Why don't the manufactures supply boards with a floating plate (hangl plate) already attached? Then you just bolt on your binding of choice and away you go. Ski manu's have been doing this for quite a while.
    I'd bet it's a cost thing, allot of the true race stock skis do not still.

    many of the plates on the skis are premounted so you're forced to use binding X
    For all your fly fishing and fly tying needs http://www.rangeleysportshop.com/

  12. #12
    Join Date
    Jan 2007
    Location
    Albany, NY
    Posts
    667
    i agree with Kirk, that would be awesome.

    i spent most of the morning looking into different materials supplied through a local distributor. i may make some inquiries into a couple of them to test them out. but if lexan works just fine then that will probably be the way to go.

    thanks for all the input so far.

  13. #13
    Join Date
    Nov 2003
    Location
    A bridge too far (the Netherlands)
    Posts
    1,559

    Boards including standard plates

    Quote Originally Posted by MUD
    My question is: Why don't the manufactures supply boards with a floating plate (hangl plate) already attached? Then you just bolt on your binding of choice and away you go. Ski manu's have been doing this for quite a while.
    For instance TINKLER or Apex board including plate

  14. #14
    Join Date
    Dec 2005
    Location
    Roseville, MN
    Posts
    1,238
    Quote Originally Posted by Hans
    For instance TINKLER or Apex board including plate
    Exactly.
    I just started my own thread on this...... Just so we don't highjack this one.
    Doug in MN

  15. #15
    Join Date
    Feb 2005
    Location
    too far south
    Posts
    3,737
    what we really need is another 50 threads on the same subject..you'd think there was no snow on the ground...


    World's foremost apres-skier, 20 years running

  16. #16
    Join Date
    Dec 2005
    Location
    Roseville, MN
    Posts
    1,238
    None here!!!!! We won't be on the snow until Thanksgiving, if that.
    Doug in MN

  17. #17
    Join Date
    Nov 2003
    Location
    Finland
    Posts
    1,247
    Quote Originally Posted by MUD
    None here!!!!! We won't be on the snow until Thanksgiving, if that.
    This was view from cabin window on crowded Saturday
    http://www.flegmatic-carving.com/gal...album=11&pos=2
    Unfortunately now i need to wait 4 weeks to get back on snow, if we dont get real cold front here sooner.

  18. #18
    Join Date
    Dec 2005
    Location
    Roseville, MN
    Posts
    1,238
    Quote Originally Posted by pokkis
    This was view from cabin window on crowded Saturday
    http://www.flegmatic-carving.com/gal...album=11&pos=2
    Unfortunately now i need to wait 4 weeks to get back on snow, if we dont get real cold front here sooner.
    NICE!!!! It is very brown here right now..... We did have some flurries about an hour ago.
    Doug in MN

  19. #19
    Join Date
    Nov 2003
    Location
    The moose's maw rangeley, me
    Posts
    6,178
    that's one shiny sexy beast of a board
    For all your fly fishing and fly tying needs http://www.rangeleysportshop.com/

  20. #20
    Join Date
    Nov 2003
    Location
    Big Utah country in them hills
    Posts
    1,431
    Quote Originally Posted by BlueB
    Bordy,
    I really think you should refrain from calling the pads Plex. It gives the wrong impression that they should be made out of Plexiglass (acrylic) insead of Lexan (polycarbonate). As discussed before, Plexiglass is a brittle material, it shatters and doesn't like compression loads araund drilled holes, nor tightening with the screws.
    Lexan or other polycarbonates are flexier and practically indestructable.

    On the side note, did anyone try the cutting board (high-molecular polyethilene). It should have nice dumping properties too...
    Product reads PLGA 220 on it I assume it is Plexaglass I am sure there are better materails to use but I have used PLEX pads for 3 season and never broken one.

    I have scene ABS used, cutting boards, Stacks of base,

    Prof is in the pudding using PLGA 220 for 3 season, Made several other sets for competing riders using same stuff, no problems.

    Since it sounds like lexan is better maybe I'll try it next time.

    How many Plates have you made?? and out of what?? how did they work?
    Hardbooter.com



    “Yes, it is much more challenging to ski 210 cm toothpicks. But do you choose to go to the wooden outhouse in the wintertime? Or it is more pleasant to use the indoor toilet instead? Why take challenges from the past when we can go on and challenge us on what’s possible with the current technology?”

    Shane McConkey disscussing rockered skis.

  21. #21
    Join Date
    Nov 2003
    Location
    Toronto, ON
    Posts
    2,287
    Dave:

    What exactly is the S-flex? $429 seems awfully dear for a plastic or rubber plate. There's got to be more to it than that. Do you have any kind of exploded view or schematic?

    Henry

  22. #22
    Join Date
    Jan 2007
    Location
    Albany, NY
    Posts
    667
    skategoat, check here..

    http://www.bomberonline.com/VBulleti...ighlight=sflex


    a note on ABS. anyone that is thinking this route should be careful with abs. it sometimes has a relatively high coefficient of thermal expansion (unlike polycarbonates). in otherwords, temperature changes could have significant impact on shrinkage and expansion of ABS plates.

  23. #23
    Join Date
    Jan 2005
    Location
    Vancouver, BC, Canada
    Posts
    4,354
    Quote Originally Posted by Bordy
    Product reads PLGA 220 on it I assume it is Plexaglass I am sure there are better materails to use but I have used PLEX pads for 3 season and never broken one.

    I have scene ABS used, cutting boards, Stacks of base,

    Prof is in the pudding using PLGA 220 for 3 season, Made several other sets for competing riders using same stuff, no problems.

    Since it sounds like lexan is better maybe I'll try it next time.

    How many Plates have you made?? and out of what?? how did they work?
    Abreviation does sound like plexiglass, indeed. Just, let's not assume, as the pros do not assume. Who is the manufacturer? That would alow one to use the product code and trace the material properties.
    3 season without failure sounds very good.

    As for me, I didn't make any plates as I didn't need any so far. However, as an industrial designer with 15 years of experience with plastic, metal and composite products, I extensivelly used acrylics and polycarbonates for products ranging from signage and safety screens up to the speed boat winshields and super yacht windows... Acrylic (Plexiglass) did fail in many situations.
    So, if one is already going through trouble of making the pads, he might as well use the material that certainly will not fail.
    INSTRUCTION | CASI L2 - hard boots all the way! | Vancouver Carvers' Diaries 2012/13 | Items for sale

  24. #24
    Join Date
    Nov 2003
    Location
    Layton, UT
    Posts
    778
    Quote Originally Posted by Bordy
    Product reads PLGA 220 on it I assume it is Plexaglass I am sure there are better materails to use but I have used PLEX pads for 3 season and never broken one.
    Thickness?

  25. #25
    Join Date
    Nov 2006
    Location
    Cadillac, MI
    Posts
    1,885
    Also ABS tends to get brittle when cold, depending on the mix.

    On another note, some board makers are using ABS for the sidewall materials, so I guess it could probably go either way.
    Soft bootin it since winter of 1998 (or sometime close)
    Hard bootin it since December 2006.

    No trees were killed in the sending of this message, but a large number of electrons were terribly inconvenienced.

  26. #26
    Join Date
    Nov 2003
    Location
    Big Utah country in them hills
    Posts
    1,431

    sorry Kirk

    Quote Originally Posted by Kirk
    Thickness?
    Sorry buddy, I ment to post it last post for ya, It about 3/16 I can't find my metric tape right now.

    BlueB,

    You sound like the guy to find out what the best commonly avalable materal may be, You mentioned lexon before, anything else? Just looking for function it is just a spacer really and the compresion force it receives is just hand turned screw pressure.

    The only other info on the Plex I am using is the sku from home depot, it reads 7450799308
    Hardbooter.com



    “Yes, it is much more challenging to ski 210 cm toothpicks. But do you choose to go to the wooden outhouse in the wintertime? Or it is more pleasant to use the indoor toilet instead? Why take challenges from the past when we can go on and challenge us on what’s possible with the current technology?”

    Shane McConkey disscussing rockered skis.

  27. #27
    Join Date
    Nov 2003
    Location
    Layton, UT
    Posts
    778
    Quote Originally Posted by Bordy
    It about 3/16 I can't find my metric tape right now.
    Thanks!

    Works out to be just under 5mm

  28. #28
    Join Date
    Sep 2005
    Location
    Hell
    Posts
    3,672
    why would it even need to be that thick? wouldnt pretty much anything that flexes and provides a buffer between binding base and board topsheet work?

    this all seems like way too much trouble for anyone but someone with disposable income.
    If death leads to eternal bliss why are you wearing a seatbelt?

  29. #29
    Join Date
    Nov 2003
    Location
    Big Utah country in them hills
    Posts
    1,431

    naw

    Dave it needs to be thick enough to disstribute the pressure over a larger area.

    What do you mean trouble its like 10 bucks and may save your board from breaking and you getting hurt.

    Since my income was $0.00 last year I will still spent it.

    I just looked at Catek they want 80 bones for a set
    Last edited by Bordy; November 5th, 2007 at 02:00 PM.
    Hardbooter.com



    “Yes, it is much more challenging to ski 210 cm toothpicks. But do you choose to go to the wooden outhouse in the wintertime? Or it is more pleasant to use the indoor toilet instead? Why take challenges from the past when we can go on and challenge us on what’s possible with the current technology?”

    Shane McConkey disscussing rockered skis.

  30. #30
    Join Date
    Sep 2005
    Location
    Hell
    Posts
    3,672
    $80? for some PLASTIC? jesus

    I mean more that the metal boards seem, IN MY OPINION kinda stupid for a recreational rider. The simple fact that you have to use spacers means there's a problem with board/binding compatibility and someone should work on it

    I guess metal is "the s--t" but at $1000+ for a board that is fragile and needs all this special care I just think it goes beyond reasonable, kinda likea 285cm board.
    If death leads to eternal bliss why are you wearing a seatbelt?

Page 1 of 4 1234 LastLast

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •